Method for manufacture of catalyst used for reduction of nitrogen oxides and the catalyst produced by the method
Abstract
A catalyst having high activity at a low temperature is obtained by heating rhodochrosite in air at a temperature of 300°-500° C. A catalyst having still higher activity at a low temperature is obtained by mixing rhodochrosite with a specific amount of a specific metal compound and heating the resultant mixture in air at a temperature of 300°-500° C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 10.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A method for the manufacture of a catalyst for use in the reduction of nitrogen oxides, which method comprises heating rhodochrosite in air at a temperature in the range of from 300° C. to 500° C.
- Claim 2Depends on #1
The method according to claim 1, wherein the heating is continued until emission of carbon dioxide gas from the rhodochrosite substantially ceases.
- Claim 3Independent Claim
A method for the manufacture of a catalyst for use in the reduction of nitrogen oxides, which method comprises: (a) mixing rhodochrosite and 1 to 80% by weight, based on the weight of said rhodochrosite, of a compound selected from the group consisting of the oxides of Fe, Ni, Cr, Co, Cu, Zn, Sn, Ti, V and W or of at least one compound which is converted into an oxide or oxy-hydrate when heated in air at a temperature in the range of from 300° C. to 500° C.; and (b)
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (10 of 10 total)
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 1,937,488 A | Manganese dioxide | 1933 | 20 |
| US 3,880,982 A | Process for removing nitrogen oxides from exhaust gases | 1975 | 12 |