Process for producing tantalum and columbium powder
Abstract
A method of producing tantalum or columbium powder is described for producing a selected desired particle size powder under controlled conditions with a high rate of production and yield of usable powder. A molten salt bath of an alkali metal tantalum fluoride or an alkali metal columbium fluoride and a relatively large amount of diluent salt to act as a heat sink is initially maintained at a low temperature in the liquidus range, an addition of liquid alkali metal reducing metal is added at a very fast rate to the continuously stirred bath to create a rapid temperature rise to the reaction temperature, and liquid alkali metal is thereafter fed at a fast rate to complete the reaction quickly at the final reaction temperature. Cooling is used for at least a portion of the reaction cycle at a rate sufficient to maintain the final reaction temperature within a desired range.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 155.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
The process of producing a metal powder of the group consisting of tantalum and columbium powders which comprises maintaining a liquid bath of a double salt of the formula R.sub.2 MX.sub.7 wherein R is an alkali metal, M is a metal of the group consisting of tantalum or columbium and X is a halogen atom of the group consisting of fluorine, chlorine, or bromine, and a diluent comprising an alkali metal halide at a temperature above the liquidus temperature of said salt mixture but not exceeding 760° C. in a closed reaction vessel, adding a molten alkali metal to said bath at a rate of at
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 155 total)
References Cited — Backward Prior Art (4)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 2,950,185 A | Production of tantalum powder | 1960 | 53 |
| US 3,829,310 A | High surface area valve metal powder | 1974 | 38 |
| US 3,992,192 A | Metal powder production | 1976 | 20 |
| US 4,067,736 A | Metal powder production | 1978 | 29 |