Patents
US 4,148,949 A#7642420 Most CitedExpiredUnited States (USPTO)Utility

Method of increasing polymerization reaction rates in the production of a fiber-thermoplastic matrix by in situ bulk polymerization

13Forward Citations (#7642420 Global)
0.3/yrCitation Velocity (#27090625 Global)
2.36Citation PageRank (#11164020 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of increasing polymerization reaction rates during the production of a fiber-thermoplastic matrix by in situ bulk polymerization is described, allowing polymerization to at least 25% polymer content by weight of the matrix in less than 8 minutes. In a fibrous web of less than 0.25-inch thickness, saturated with a liquid phase polymerizable composition containing a vinyl monomer and a thermally activated free radical initiator at 1/2-10% by weight of the composition, polymerized by the application of controlled temperature and pressure conditions, reaction rates of less than 8 minutes are attained by: (a) initiating polymerization with the matrix containing a monomer concentration in excess of that which if completely polymerized is desired in the final product matrix; and (b) polymerizing the monomer contained in the matrix until the desired level of polymer is attained while, simultaneously with the polymerizing step, removing excess monomer at a controlled rate such that the reaction is sustained until the desired level of polymer in the finished matrix is attained. The resulting matrix is then treated further to remove any excess monomer and is suitable for molding by t

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 13.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    In a method for the production of a moldable, fiber-thermoplastic polymer matrix wherein a fibrous web of less than 0.25-inch thickness and of less than 600 lbs./3,000 ft 2 basis weight is saturated with a liquid-phase composition, comprising a vinyl monomer and a thermally activated polymerization initiator in an amount of 0.5-10% of said composition having a viscosity of less than about 10,000 centipoise, is subjected to heat and results in a matrix comprising at least about 25% polymer by weight of said matrix, the improvement wherein polymerization time is less than eight minutes, compris

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Beall, F. C. et al., Direct and RF Heating Curing of Wood-Plastic Composites, Forest Product, Journal, vol. 16, No. 9, Sep. 1966, pp. 99-106.