Production of aluminum polyphosphate
Abstract
Aluminum polyphosphate is made. To this end, solid aluminum hydroxide and polyphosphoric acid which are used in proportions corresponding to an Al:P molar ratio of 1:2.5 to 1:3.5, are introduced separately from, but concurrently with, one another into a reaction zone kept at 150° to 200° C. A moist friable consistency of the starting materials is maintained in the reaction zone by continuously mixing, kneading and comminuting them over substantially the entire period during which they are introduced into the reaction zone. The reaction is continued until a dry sandy powder is formed; and the powder is annealed at 400° to 600° C. over a period sufficient to yield a product undergoing a 0.5 to 1% weight loss on ignition.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 35.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A process of producing long chain aluminium polyphosphates as defined in ASTM 13-266, which comprises step (A) of introducing into a reaction zone as starting materials aluminum hydroxide and polyphosphoric acid containing 75 to 85 weight % of P 2 O 5 in amounts corresponding to a molar ratio of Al:P of 1:2.5 to 1:3.5; continuously mixing, kneading and comminuting the starting materials in the reaction zone and heating the resulting mixture at a temperature of 150° to 200° C. for as long as necessary to ensure conversion to a dry, sandy, pulverulent intermediate product; and step (B) of dehy
- Claim 2Depends on #1
The process as claimed in claim 1, wherein the proportio