Graft modified polyethylene process and product
Abstract
A graft modified polyethylene process is described which comprises contacting polyethylene with an organic peroxide in the presence of an ethylenically unsaturated polycarboxylic acid or derivative thereof at a temperature of from 140°-210° C. The resulting graft modified polyethylene in combination with polyamides provide polymer blends having improved impact properties.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 53.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A process which comprises, mixing polyethylene with from 0.1 to 1.5% by weight, based on the weight of unmodified polyethylene, of an ethylenically unsaturated polycarboxylic acid anhydride modifier, under melt conditions at a temperature within the range of from 140° C. to 210° C. in the presence of an organic peroxide having a half life of at least about 60 seconds within said temperature range whereby substantially all of said modifier is grafted onto the polyethylene backbone to produce a graft modified polyethylene, said graft modified polyethylene having a melt viscosity greater than the
- Claim 2Depends on #1
A process in accordance with claim 1, where the modifier is an ethylenically unsaturated anhydride of the formula, ##STR10## w