Method for producing colored anodic oxide films on aluminum based alloy materials
Abstract
Method for producing colored anodic oxide films on aluminum-based alloy materials comprising steps of subjecting the material having an oxide film thereon to a coloring electrolytic treatment in a bath of electrolyte containing water soluble nickel salt and boric acid. The material is applied with alternating voltage pulses having negative pulse duration which is the same as or greater than duration of positive voltage pulse.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 8.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for producing coloured oxide films comprising subjecting an aluminum based material to an anodizing treatment to produce an oxide film thereon, dipping the material in an electrolyte bath containing from about 70 to about 150 grams of water-soluble nickel salt per liter of water and from about 20 to about 50 grams of boric acid per liter of water, wherein the bath is maintained at a temperature between about 20° and about 22° C., and applying alternating voltage pulses to the aluminum based material, the alternating voltage pulses including more than one negative voltage pulse and mor
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗