Abstract

A crosslinked, soft, flexible, closed-cell foam of chlorinated high density polyethylene and a process for the preparation thereof, comprising admixing a high density chlorinated polyethylene with a thermally decomposable chemical foaming agent at a temperature below the decomposition temperature of said foaming agent, molding the chlorinated high density polyethylene into desired form at a temperature below the decomposition temperature of the foaming agent, subjecting the molded chlorinated high density polyethylene to irradiation crosslinking at a temperature below the decomposition temperature of said foaming agent and contacting, in a substantially oxygen-free environment, the crosslinked chlorinated high density polyethylene with a heat transfer medium maintained at a temperature of from about 150° C. to about 350° C. for a period sufficient to form the desired product.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 10.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for preparing a crosslinked, soft, flexible, closed-cell foam from chlorinated high density polyethylene said foam having a cell size of from about 0.05 to about 2 mm, a density of from about 2.5 to about 50 pcf, a tensile strength of from about 30 to about 600 psi, and a tensile elongation of from about 200 to about 500 percent, said process comprising (a) preparing a foamable mixture by mixing a suspension chlorinated high density polyethylene containing from 25 to about 48 percent of chemically combined chlorine and having a flexural modulus at 25° C. of less than about 15,000 psi