Patents
US 4,140,740 A#6138381 Most CitedExpiredUnited States (USPTO)Utility

Flatness control of thermoplastic film

15Forward Citations (#6138381 Global)
0.3/yrCitation Velocity (#24772991 Global)
3.61Citation PageRank (#5626176 Global)
6Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method for the production of biaxially molecularly oriented polymeric film, wherein the flatness of the film is improved by subjecting the film preferably immediately after its heat-setting to a longitudinal tension that is at least three times higher than the normal film transport tension in the production process. Preferably, said higher longitudinal tension is at least 100 kp/sq.cm. The film may be subjected also between its longitudinal stretching and its heat-setting to said at least three times higher longitudinal tension. The temperature of the film during said treatment at increased longitudinal tension is between room temperature and the second order transition temperature of the film.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 15.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    Method for continuously producing molecularly oriented heat set polymer film, comprising the steps of extruding a linear organic, crystallizable thermoplastic polymer to form a molten layer and quenching said layer to obtain a substantially amorphous film, biaxially molecularly orienting said film by longitudinally and transversely stretching the film at a film temperature between the second order transition temperature of the polymer and about 50° C. above said transition temperature, heat setting the oriented film by heating the film to a temperature within a range of about 25° C. above

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗