Low cost method of fluidizing cupola slag (A)
Abstract
A method of fluxing and fluidizing the slag in a cupola by adding to the charge therein a fluxing material comprising, by weight percentage relative to the metal charge, 3-5% CaCo 3 (limestone), 3-5% MgCO 3 . CaCO 3 (dolomite), and 1-2% Na 2 CO 3 (fused soda ash). This fluxing and fluidizing material is used for operating a basic cupola and is used in amounts ranging from about 7 to 12 by weight of the metal charge. The flux material serves to remove impurities from the metal, and improve the combustion efficiency of the coke. In an acid slag cupola, the flux will increase fluidity. In a basic slag, a fluidizer serves to improve the fluidity of the slag, while offering no injurious by-products that would interfere with emission control elements, and additionally insures a lower cost fluxing material as compared to current basic operated cupola practices.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 10.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of fluxing slag in a basic operated cupola for making low sulfur and/or high carbon irons, by adding to the cupola charge therein an effective amount of fluxing materials comprising, by weight in the slag analysis 45-55% CaO, 9-15% MgO, 2-4% Na 2 O, about 6.5% Al 2 O 3 , about 23-33% SiO 2 , and less than 0.2% CaF 2 .
- Claim 2Depends on #1
The method as in claim 1, in which the fluxing materials constitute about 2.5-12% by weight of the total metal charge for said cupola.
- Claim 3Depends on #1
The method as in claim 1, in which the fluxing materials are effective to obtain a viscosity for the resultant slag which is at least as fluid as 500 cps at operating temperatures and has a fusion temperature which is at least 2300° F.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (10 of 10 total)
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 1,590,730 A | Method of desulphurizing iron | 1926 | 12 |
| US 1,963,269 A | Method of desulphurizing and purifying iron | 1934 | 5 |