Glass-ceramic composition for hermetic seals
Abstract
The invention relates to a glass-ceramic composition having a high fracture strength adaptable for hermetically sealing to chromium bearing iron or nickel base alloys at temperatures of between about 950° C to about 1100° C to form a hermetically sealed insulator body, comprising from about 55 to about 65 weight percent SiO 2 , from about 0 to about 5 weight percent Al 2 O 3 , from about 6 to about 11 weight % Li 2 O, from about 25 to about 32 weight percent BaO, from about 0.5 to about 1.0 weight percent CoO and from about 1.5 to about 3.5 weight percent P 2 O 5 .
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 20.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A glass-ceramic of high fracture strength for sealing to chromium bearing iron or nickel base alloys, comprising from about 55 to about 65 weight percent silicon dioxide, from about 0 to about 5 weight percent aluminum oxide, from about 6 to about 11 weight percent lithium oxide, from about 25 to about 32 weight percent barium oxide, from about 0.5 to about 1.0 weight percent cobalt oxide, and from about 1.5 to about 3.5 weight percent phosphorous pentoxide.
- Claim 2Depends on #1
The glass-ceramic of claim 1 wherein said silicon dioxide is about 60 weight percent, said lithium oxide is about 9 weight percent, said barium oxide is about 28.5 weight percent, said cobalt oxide is about 0.5 weight percent, and said phosphorous pentoxide is about 2 weight percent.
- Claim 3Depends on #1
The glass-ceramic of claim 1 having a thermal expansion coefficient of about 1.0