Roast-reductive leach process for copper recovery

18Forward Citations (#4860380 Global)
0.4/yrCitation Velocity (#20911702 Global)
3.53Citation PageRank (#5827952 Global)
9Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A sulfide containing copper and one or more of iron, nickel and cobalt, is dead-roasted at a temperature of 750° C or above, then subjected to a pressure leach under reducing conditions to produce elemental copper and an aqueous solution of the other metals.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 18.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for recovering copper from a particulate sulfide-containing material which contains in addition to said copper at least one other metal selected from the group consisting of iron, nickel and cobalt, comprising roasting said material at a temperature of at least about 750° C. for a period of sufficient duration to provide a substantially sulfur-free calcine, forming a slurry of said calcine with water or an aqueous solution containing at least a sufficient amount of sulfuric acid to supplement any sulfuric acid formed in situ and satisfy the stoichiometry of formation of sulfates of s

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Shirts et al., Bureau of Mines Report of Investigations 7996, (1975).