Patents
US 4,134,528 A#10638170 Most CitedExpiredUnited States (USPTO)Utility

Method of producing copper clad steel wire

10Forward Citations (#10638170 Global)
0.2/yrCitation Velocity (#32071453 Global)
1.88Citation PageRank (#16071113 Global)
4Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Copper-clad steel wire is produced by forming a copper tube around the wire, and drawing down the copper tube and wire to reduce the cross-section of the wire by at least 30%. The wire is annealed, slowly cooled and the cross-section further reduced by at least 10%.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 10.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of producing copper-clad steel wire, comprising: providing a copper tube around a steel wire, said tube having an inside diameter larger than the outside diameter of the steel wire; reducing the cross section in the cold state by at least 30% followed by annealing at at least 800° C. for at least 3 hours, slow cooling and reduction in cross-section in the cold state by at least 10%.

  2. Claim 2Depends on #1

    A method according to claim 1, wherein the wire is first reduced in cross-section by at least 50% in a plurality of drawing stages, thereupon annealed at from 830° C. to 870° C. for from 3 to 4 hours in vacuo or in an atmosphere of protective gas, slowly cooled in vacuo or in an atmosphere of protective gas and finally reduced in cross-section by at least 30% in the cold state in a plurality of passes.

  3. Claim 3Independent Claim

    A method acc

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗