Patents
US 4,133,669 A#2251764 Most CitedExpiredUnited States (USPTO)Utility

Process for pelletizing a sulphur-bentonite clay mixture and the product formed thereby

30Forward Citations (#2251764 Global)
0.6/yrCitation Velocity (#12257129 Global)
5.46Citation PageRank (#2870330 Global)
5Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A process for pelletizing a mixture of elemental sulphur and bentonite clay to produce a water degradable prill includes adding dry clay dust to molten sulphur at an elevated temperature to provide a molten sulphur-clay mixture, forming droplets of the mixture, providing a liquid fertilizer coolant at a temperature lower than the freezing temperature of the sulphur-bentonite mixture, feeding the droplets into the coolant, passing the droplets through the coolant for a time sufficient to anneal the droplets into pellets, and removing the annealed pellets from the coolant.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 30.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for the manufacture of solid pellets of a water-degradable solid suspension of bentonite clay in elemental sulphur, comprising the steps of: adding one to three parts (out of ten parts) of substantially dry clay dust to seven to nine parts of molten sulphur with continuous and thorough mixing in a mix-tank at an elevated temperature between 238° F. and 300° F.; forming droplets of the mixture; providing a nitrogen containing liquid fertilizer solution, said solution containing a non-degrading amount of water; feeding said droplets into said liquid fertilizer soltuion; passing

  2. Claim 2Depends on #1

    The process according to claim 1 wherein said liqu

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗