Treatment of acrylamide polymer gel
Abstract
A method for reducing the amount of water-insolubles and free monomer in an aqueous acrylamide polymer gel whereby the gel is heated at from about 80 DEG C to about 150 DEG C for at least about 30 minutes while the water content of the gel is maintained substantially constant.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 8.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for the reduction of the amount of water insolubles and free monomer in an aqueous acrylamide polymer gel charge containing at least about 25% polymer and having a molecular weight of at least about 4 million which comprises heating said polymer gel, in the substantial absence of a sulfite compound, at a temperature ranging from about 80° C. to about 150° C. for at least about 30 minutes while simultaneously maintaining the water content of the gel undergoing heating at substantially the concentration of that of said charge and recovering the resultant polymer gel.
- Claim 2Depends on #1
A method according to claim 1 wherein the recovered polymer gel is dried.
- Claim 3Depends on #1
A method according to claim 1 wherein the recovered polymer gel is granulated and dried.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗