Patents
US 4,131,444 A#22513852 Most CitedExpiredUnited States (USPTO)Utility

Method for increasing the strength and density of lead titanate ceramic bodies

4Forward Citations (#22513852 Global)
0.1/yrCitation Velocity (#47827232 Global)
7.78Citation PageRank (#1610197 Global)
9Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Strengthened and densified ceramic bodies are produced by hot pressing lead titanate powder into a lead titanate ceramic at a pressure from 1000 to 5000 psi and at a temperature from 700 to 1100 DEG C if the atmosphere is reducing or from 700 to 1200 DEG C if the atmosphere is oxidizing and by annealing the lead titanate ceramic at a temperature from 600 to 1100 DEG C in an oxidizing atmosphere for at least four hours.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 4.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for producing a lead titanate ceramic from a lead titanate composition susceptible to Curie-point degradation which comprises hot-pressing a lead titanate composition comprising at least 98 weight percent of lead titanate with no other constituent in excess of one weight percent to form a lead titanate ceramic at a pressure from 1000 to 9000 psi and at a temperature from 700° C. to 1100° C. if said lead titanate is in a reducing atmosphere or at a temperature from 700° to 1200° C. if said lead titanate is in an oxidizing atmosphere; and cooling said lead titanate ceramic to room tempe

  2. Claim 2Depends on #1

    The method of claim 1 which further comprises annealing said lead titanate ceramic at a temperature from 600° C. to 1100° C. in an oxidizing atmosphere for at least fo

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗