Patents
US 4,130,698 A#1912479 Most CitedExpiredUnited States (USPTO)Utility

Polyurethane foam containing internal mold-release agent

33Forward Citations (#1912479 Global)
0.7/yrCitation Velocity (#11016422 Global)
7.39Citation PageRank (#1751533 Global)
7Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A mold-release agent is provided which consists essentially of 99.9% to 80% by weight of an aromatic polyisocyanate containing at least two isocyanate groups and 0.1% to 20% by weight of a fatty acid ester, e.g., glycerol trioleate, olive oil, peanut oil, etc. A process of using the material by incorporating it in polyurethane foams is disclosed.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 33.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for the production of polyurethane foam mouldings which comprises foaming a reaction mixture which comprises (A) an aromatic polyisocyanate containing at least two isocyanate groups, (B) at least one compound containing at least two isocyanate reactive groups, (C) a foaming agent, (D) a foam stabiliser and (E) 2% to 8% by weight based on the weight of (B) of at least one processing aid which is an ester of fatty acid containing 6 to 25 carbon atoms and an aliphatic saturated alcohol containing 2 to 4 hydroxyl groups, said reaction being carried out in a closed mould.

  2. Claim 2Depends on #1

    A process according to claim 1 in which the weight of processing aid is between 3% and 5% by weight.

  3. Claim 3Depends on #1

    A process according to claim 1 in which the processing aid is glycerol trioleate.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 33 total)

PatentTitleYearCitations
US 5,500,176 AProcess for the production of molded products using internal mold release agents199619
US 4,451,425 AMethod for injection molding polyurethane using internal release agents198417
US 4,298,556 AMethod for matched die molding a fiber reinforced polyurethane foam molded product198122
CN 1,057,781 CWaterproof plastic foam20000
US 4,383,050 AProcess for the preparation of low temperature flexible polyurethane elastomers198330
US 7,030,066 B1Wetting composition for high temperature metal surfaces, and method of making the same20060
JP 2005246964 AComposite element made of polyurethane material with surface composed of thermoplastic substance layer or metallic layer, and manufacturing method therefor—0
US 10,619,001 B2Polyurethane foam forming composition including triglycerides, polyurethane foam made from the composition, and method of making polyurethane foam20201
JP S6191216 AProduction of molded body—6
US 4,936,917 AWater based mold release compositions containing poly(siloxane-glycol) surfactants for making polyurethane foam article in a mold199021
US 5,670,553 AInternal mold release compositions199725
US 4,420,570 AReaction injection molded elastomer containing an internal mold release made by a two-stream system198325
US 4,581,387 AInternal release agents for polyisocyanate addition polymerization, their use in the preparation of cellular, microcellular, and noncellular polyurethane-polyurea molded parts having improved demolding properties198638
US 6,372,160 B1Process for using aqueous release compound20023
US 5,993,528 AInternal mold release compositions199917

Non-Patent Literature (2)

  • Saunders et al.-Polyurethanes, Part II, Interscience, N.Y. (1964), pp. 99-106.
  • U.S. Testing Co.-Tables & Data; pp. 28-29, Composition & Constants of Fats & Oils, published about 1954.