Process of applying tin oxide on glass using butyltin trichloride
Abstract
The coefficient of friction of glass is decreased and the scratch resistance is improved by applying finely divided or vaporized butyltin trichloride to the heated glass articles to produce a coating of stannic oxide on the glass. The glass is then coated with a conventional lubricating wax.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 26.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method for reducing the coefficient of friction and susceptibility to scratching exhibited by glass surfaces, the method consisting essentially of the following sequence of operations: (1) Maintaining said glass surface at a temperature of between 450 and 600° C. while applying to said glass surface vaporized or finely divided butyltin trichloride, (2) Maintaining the glass surface at a temperature of 350° C. or below while applying to the glass surface a coating of a natural wax or synthetic polymer.
- Claim 2Depends on #1
A method as described in claim 1 wherein the synthetic polymer is selected from the group consisting of polyethylene, oxidized polyethylene, copolymers of a polyoxyalkylene or etherified polyoxyalkylene and a dialkylpolysiloxane, copolymers of vinyl esters or esters of ethylenically unsaturated carboxylic acid and other ethyl
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗