Abstract

A castable slip of a bimodal distribution of silicon carbide particles is prepared, the slip preferably containing a water miscible curable resin. A shaped body is cast in a plaster of paris mold which also preferably contains a small amount of a water soluble polymer. The casting and mold are then heat treated to increase the strength of the green casting. In a preferred embodiment of the invention the resin in the slip is cured by the heat treating step. The mold is then removed by decomposing the mold material, preferably by dipping the mold in acid to attack the mold material (e.g. the water soluble polymer or the plaster of paris itself). The cured resin in the casting is sufficiently resistant to attack by the acid to survive the mold removal. In an alternative embodiment the silicon carbide body is heated to a sufficiently high temperature (e.g. 650°-750° C) to slightly oxidize the SiC and to strengthen the green casting. Along with this heating the water soluble polymer in the mold is burned out and the mold is thereby weakened to permit its ready removal. Thereafter, the cast silicon carbide product is fired to carbonize any resin in the SiC and recrystallize the silicon c

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 18.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for casting a complex silicon carbide shape which requires destruction of the mold to permit removal of the complex cast shape, said process including the steps of forming a castable aqueous slip from particles of finely powdered silicon carbide, said slip containing approximately 1 to 10% of a water miscible resin that will set or cure at a temperature below 200° C. to a structure that is relatively inert to an acid, casting said slip into a plaster mold which is attacked by said acid, heat treating the mold and cast slip to cure said resin and increase the green strength of the cas