Process for making fiber-forming polyesters
Abstract
A flame-retardant, easily dyeable polyester and the process for preparing the same by polycondensing a glycol phthalate prepolymer with a phosphine oxide and dye improver selected from the group consisting of R--O(G--O).sub.x --H where R is an alkyl group containing an average of from about 8 to about 20 carbon atoms; G is a hydrocarbon radical selected from the group consisting of ethylene, propylene, butylene and isomers thereof, and mixtures of the above, and x has a value of about 8-20, and ##STR1## where R is O, (CH 3 ) 2 or H 2 and the sum of x and y is 4-30. The polymer will be made up of 82 to 98 weight percent of the prepolymer, 8 to 1 weight percent of the dyeability improver and 10-1 weight percent of the phosphine oxide and is preferably formed in the presence of a catalyst which is the reaction product of germanium dioxide and a tetraalkyl ammonium hydroxide.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 5.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A flame retardant and easily dyeable fiber-forming polyester polymer containing (A) 82-98 weight percent ethylene terephthalate; (B) 8 to 1 weight percent of a dyeability improver selected from the group consisting of R--O(G--O).sub.x --H where R is an alkyl group containing from about 8 to about 20 carbon atoms; G is a hydrocarbon radical selected from the group consisting of ethylene, propylene, butylene and isomers thereof, and mixtures of the above, and x has a value of about 8-20, and ##STR8## where R is O, (CH 3 ) 2 or H 2 and the sum of x and y is 4-30, and; (C) 10 to 1 weight p
- Claim 2Depends on #1
The polymer of claim 1 wherein the dyeability improver is selected from the group
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗