Abstract

Environmentally stable bond joints of aluminum metal and aluminum alloys in adhesively joined structures are formed by utilizing a prebonding anodization of the aluminum surfaces in a phosphoric acid electrolyte using an electrolyte bath temperature of 60° to 85° F. The anodized surface is then removed from the electrolyte bath and washed free of electrolyte within from one half to two and one half minutes from cessation of anodizing current, dried and coated with adhesive resin. The anodized aluminum metal surfaces are then juxtaposed with an adhesive resin and bonded together under pressure and heat to cure the adhesive resin. The resulting structure is resistant to failure of the bond joints on exposure to moist atmospheric conditions. The surface preparation provides a porous hydration resistant aluminum oxide surface which minimizes adhesive failure to the oxide-adhesive interface under aqeuous exposure. Alloys containing copper and other constituents may be successfully anodized and bonded by this process.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 38.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of preparing an adhesively bonded aluminum structure comprising: forming a porous columnar aluminum oxide coating on surfaces of aluminum alloy articles by anodizing said articles in an aqueous solution comprising phosphoric acid, the anodizing potential being from about 3 to about 25 volts, the phosphoric acid concentration being about 3 to about 20% by weight and the temperature of said solution being about 50° F. to about 85° F.; rinsing said articles to remove said solution within 0.5 to 2.5 minutes from cessation of anodizing current; bonding said aluminum articles together t

  2. Claim 2Depends on #1

    The method of claim 1, wherein the thickness of said porous coating is from about 500 to about 8,000 Angstroms.

  3. Claim 3Depends on #2

    The method of claim 2, wherein said coating has pores leaving a diameter

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (0)

No backward patent references recorded.

Non-Patent Literature (1)

  • "The Surface Treatment of Al and its Alloys", by S. Wernick et al., 1964, p. 597.