Patents
US 4,126,522 A#3048683 Most CitedExpiredUnited States (USPTO)Utility

Method of preparing aluminum wire for electrical conductors

25Forward Citations (#3048683 Global)
0.5/yrCitation Velocity (#15032247 Global)
3.60Citation PageRank (#5641603 Global)
2Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Aluminum wire, of either pure aluminum or an aluminum alloy is plated with a firm layer of nickel by passing the wire through a pickling bath of an aqueous solution of phosphoric and hydrochloric acids at a temperature of between 50° and 70° C and then electroplating the wire with nickel.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 25.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    The method of preparing an aluminum wire for subsequent nickel plating for electrical conductors comprising passing the wire through an acid bath consisting of an aqueous solution containing 20 -35% by volume of 35% hydrochloric acid and 5 -13% by volume of 85% phosphoric acid, said bath having a temperature of between 50° and 70° C.

  2. Claim 2Depends on #1

    The method of claim 1 further comprising the step of electroplating nickel on the surface of the aluminum wire after it has passed through the acid bath.

  3. Claim 3Depends on #2

    The method of claim 2 wherein the volume of the hydrochloric acid is 30%, the volume of the phosphoric acid is 10%, the volume of water is 60% and the temperature is 60° C.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (2)

Non-Patent Literature (1)

  • "Cleaning and Etching Aluminum," S. Spring; Metal Finishing, Aug. 1968, p. 6671.