Producing improved metal alloy products (Al-Fe alloy and Al-Fe-Si alloy)
Abstract
A dispersion strengthened aluminum alloy sheet is produced by casting an Al-Fe 1.1 - 2.5% alloy optionally containing Si up to 2.0% and, optionally, proportions of other specified alloying constituents. The alloy is cast in the form of a slab at a growth rate in excess of 25 cm/min. at a thickness of less than 25 mm so that intermetallics are formed in the slab in the form of fine rods of a diameter of 0.05 - 0.5 micron. These rods are then segmented by reducing the slab by at least 60% by rolling to develop a dispersion of fine intermetallic particles. By final annealing the rolled sheet at a temperature in the range of 250° - 400° C a sheet having a good combination of yield strength and formability is obtained (as indicated by a yield strength of greater than 15 k.s.i. and tensile elongation greater than 15%).
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 17.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of producing an aluminum alloy sheet product from an Al-Fe binary, ternary or higher order alloy which comprises casting the alloy in the form of a slab of a thickness less than 25 mm at a growth rate in excess of 25 cm/min. for depositing intermetallics in the form of elongated rods in a size range of 0.05-0.5 microns diameter, subjecting the cast slab to at least 60% reduction by rolling for fragmenting the intermetallic rods, said rolled sheet being subjected to final annealing at a temperature in the range of 250-400° C., for producing sheet having a yield strength greater than 15
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗