Solution and procedure for depositing a protective precoating on surfaces of zinc-coated ferrous metal parts against corrosion in presence of water
Abstract
Solution and procedure of depositing a coating on the surfaces of zinc-coated ferrous metal parts which protects against corrosion in the presence of water. The solution is made up by adding to water, perliter of final solution, of 1 to 40 grams of sodium metasilicate, 14 to 40 milliliters of phosphoric acid, specific gravity 1.71, from 1 to 40 grams of sodium nitrate, from 10 to 50 grams of anhydrous zinc chloride and the pH is adjusted to a value between 2.3 and 3.8. Preferably nickel chloride is added. For use, the solution is heated to a temperature ranging from 15° to 75° C and brought into contact with the parts to be treated for a period from 20 to 72 hours. The deposit is continuous, hard, resistant to shocks and abrasion and imparts an efficient and lasting protection to galvanized parts in corrosive waters. The invention is useful for the protection of piping in the building industry.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 4.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A solution intended for depositing rapidly a coating which protects the surfaces of zinc-coated ferrous metal parts, characterized by containing water as the solvent and per liter of final solution, from 1 to 40 grams of sodium metasilicate, from 14 to 40 milliliters of phosphoric acid having a specific gravity of 1.71, from 1 to 40 grams of sodium nitrate, from 10 to 50 grams of anhydrous zinc chloride, the pH of the aforesaid solution being adjusted to a value between 2.3 and 3.8.
- Claim 2Depends on #1
A solution according to claim 1, characterized by its containing in addition up to 70 grams of sodium hexametaphosphate per liter of final solution.
- Claim 3Depends on #2
A solution according to claim 2, which contains also nickel chloride introduced before adjusting the pH of the solution in a quantity equivalent to from 0.5 to 20 grams of hexahydrated nicke
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (4 of 4 total)
References Cited — Backward Prior Art (12)
Non-Patent Literature (5)
- Hatch, Polyphosphate Inhibitors in Potable Water, Materials Protection, Nov. 1969, pp. 31-35.
- Ibid, Aug. 17, 1973, p. 42.
- Piatti, "Passivierung und Schutzschietenbildung in Aufbereiten Wassern", Korrosion X, (Verlag Chemie GmbH, Weinheim, West Germany) 1958, pp. 31-35.
- Zinc Research Digest No. 30, International Lead Zinc Research Organization, Inc., N.Y.C., Mar. 26, 1973, pp. 27 & 28.
- Zinc Research Digest No. 31.