Recovery of high purity aluminum chloride is achieved by use of a series of condensers wherein the first condenser is operated at a high temperature of 80°-110° C to insure minimum condensation of other metal chlorides such as titanium chloride, silicon chloride, or the like, while a second condenser operates at a much lower temperature of from 20°-50° C to trap all impurities while reducing the chloride losses to a minimum. The product of the first condenser may then be used as a feed for the electrolytic reduction of aluminum chloride to metallic aluminum.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    In the process for the recovery of high purity particulate aluminum chloride from a chlorinator by the condensation of hot aluminum chloride vapors the improvement which comprises: (a) introducing the aluminum chloride vapors at an entrance velocity of 18 to 90 meters/second into a first fluidized bed having a particle size range of 1-500 microns of aluminum chloride particles maintained at a temperature of 80°-110° C.; (b) controlling the size of the solid particles of aluminum chloride particles within the fluidized bed during condensation to prevent growth of the particles larger than 500

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (2)

Non-Patent Literature (1)

  • Othmer, Fluidization, 1956, pp. 125-130.