Patents
US 4,124,413 A#11001621 Most CitedExpiredUnited States (USPTO)Utility

Wear and pitting resistant cast iron

9Forward Citations (#11001621 Global)
0.2/yrCitation Velocity (#34480598 Global)
4.04Citation PageRank (#4682005 Global)
13Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Wear and pitting resistant cast iron consisting essentially of 2.8 - 3.3% carbon, 1.5 - 2.1% silicon, 1.0 - 1.5% chromium, 0.6 - 0.8% molybdenum, 0.2 - 0.5% nickel, balance substantially all iron. The free cementite in the iron in its as-cast state amounts to 20 - 40% by volume and the casting is then held at 860 DEG - 950 DEG C for 1 - 10 hours, followed by quenching, for hardening purposes.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 9.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    Wear and pitting resistant alloyed cast iron consisting essentially of: 2.8-3.3% carbon, 1.5-2.1% silicon, 1.0-1.5% chromium, 0.6-0.8% molybdenum, 0.2-0.5% nickel, not more than 0.05 phosphorus, balance essentially iron, said cast iron having a free cementite content of 20-40% by volume in its as-cast state and having been heated at 860°-950° C. for 1-10 hours after casting, and then quenched.

  2. Claim 2Depends on #1

    The cast iron of claim 1 which has been heated after casting for 1-10 hours at 860°-900° C.

  3. Claim 3Depends on #1

    The cast iron of claim 1 which has first been heated at 900°-950° C. for 1.0-1.5 hours after casting, and then quenched in oil from at ambient temperature to 150° C. after cooling to 820°-850° C.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Metals Handbook, 1948 Ed., pp. 512, 513 & 519.