US 4,124,075 A#6057849 Most CitedExpiredUnited States (USPTO)Utility

Use of oil-wetting spacers in cementing against evaporites

15Forward Citations (#6057849 Global)
0.3/yrCitation Velocity (#24996867 Global)
4.71Citation PageRank (#3653299 Global)
11Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

This specification discloses a method of cementing pipe in a well and discloses the use of a designed oil-wetting liquid and cement slurry for cementing pipe against evaporite sections penetrated by the well. The cement slurry is formulated from hydraulic cement, silica flour, ionization control agent, sodium chloride, weighting agent, dispersing and retarding agent, and water, and has a density within the range of about 15.8 to 21.0 pounds per gallon.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 15.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    In the drilling of a well with a water base drilling mud, a method of cementing pipe against an evaporite section penetrated by said well, comprising the steps of: (a) flowing an oil-wetting liquid through the annular space formed intermediate said pipe and the wall of said well to oil-wet said evaporite section; (b) forming a pumpable cement slurry comprised of hydraulic cement, sodium chloride in an amount of at least about 18 weight percent based on mixing water, an ionization control agent in an amount up to 1.5 weight percent based on cement, mixing water and weighting agent in an amoun