High speed tool steel having high toughness
Abstract
A high speed tool steel having high toughness as well as excellent wear resistance and heat resistance characteristics, this steel contains, by weight, C 0.7 - 1.4%, Si 0.5% max., Mn 0.5% max., Cr 3 - 6%, W 1 - 3.2%, Mo 5.5 - 7.5%, V 1 - 3.5%, Co 15% max., N 0.02 - 0.1%, one or more of Ti, Nb, and Zr 0.02 - 0.1% in total and the balance being Fe and incidental impurities. The relationship between tungsten and molybdenum contents of the steel is expressed in the formulated range 12% ≦ W + 2Mo ≦ 16%.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 29.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A high speed tool steel having high toughness, consisting essentially of by weight percentages, C 0.7 - 1.4%; Si 0.5% max.; Mn 0.5% max.; Cr 3 - 6%; W 1 - 3.2%, Mo 5.5 - 7.5%, and the relationship between the contents of W and Mo being 12% ≦ W + 2Mo ≦ 16%; V 1 - 3.5%; Co 15% max.; N 0.02 - 0.1%; one or more of the elements selected from the group of Ti, Nb and Zr and being 0.02 - 0.1% in total, the balance being Fe and incidental impurities.
- Claim 2Independent Claim
A high speed tool steel having high toughness, consisting essentially of by weight percentages, C 0.8 - 1.0%; Si 0.5% max.; Mn 0.5% max.; Cr 3.5 - 5%; W 1.2 - 2.5%, Mo 6.5 - 7.4%, and the relationship between the contents of W and Mo being 14.1% ≦ W + 2Mo ≦ 16%; V 1.1 - 2.0%; Co 9% max.; N 0.02 - 0.045%; either one or more of the elements selected from the group of Ti, Nb and Zr and being 0.02 - 0.045
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗