Polymers and rotationally molding same
Abstract
A composition that can be rotationally molded with a minimum formation of bubbles comprises solid polymer, a cross-linking agent, a solid pigment in an amount to provide a surface area up to 30 m 2 /100 grams of polymer, and a transition metal catalyst residue content of less than about 3 parts per million.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 26.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A composition of matter comprising a solid polymer, an acetylenic diperoxy compound and a carbon black wherein the solid polymer is selected from the group consisting of ethylene hompolymers, copolymers of ethylene and at least one acyclic mono-1 olefin hydrocarbon having 3 to 8 carbon atoms per molecule, and mixtures thereof, wherein the amount of the acetylenic diperoxy compound is a crosslinking amount and the acetylenic diperoxy compound is selected from the group consisting of hexynes having the formula ##STR3## octynes having the formula ##STR4## and octadiynes having the formula ##STR
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 26 total)
References Cited — Backward Prior Art (4)
Non-Patent Literature (1)
- Williams et al., Tech. Ser. Report., "The Effect of the Chemical and Physical Properties of Carbon Black on its Performance in Polyethylene", Cabot Corp. 1963, pp. 38-41.