Patents
US 4,104,445 A#6681254 Most CitedExpiredUnited States (USPTO)Utility

Method for making steel wire

14Forward Citations (#6681254 Global)
0.3/yrCitation Velocity (#25935782 Global)
3.65Citation PageRank (#5521192 Global)
3Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method for making filamentary steel wire from particulate iron oxides with the aid of a fiber-forming acrylic polymer is disclosed. A precursor filament is first formed by wet-spinning an acrylic polymer spin dope in which particles of iron oxide are dispersed. The resulting precursor filament is then exposed to a reducing atmosphere (e.g., a gaseous mixture of hydrogen and carbon monoxide) at a temperature in the range of from about 900° C. to 1150° C. for a period of about 3 to 8 minutes. Under these conditions, the iron oxide particles are reduced to the metallic state and the polymer in the precursor is pyrolized to carbon and byproduct gases. The carbon diffuses into the resulting metallic iron, and the individual metal particles sinter to form continuous steel wire. The method has the capability of producing steel wire of an essentially ferritic/pearlitic structure with a tensile property in excess of 140,000 psi. When the product is converted to a tempered martensite structure tensile strengths exceeding 260,000 psi are achievable.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 14.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for producing filamentary steel wire wherein particles of iron oxide are combined with a fiber-forming acrylic polymer to first form a precursor filament which is then converted to steel wire, said method comprising the following steps in sequence: (A) providing a spinning dope wherein particles of iron oxide having an average diameter of about 5 microns or less are uniformly dispersed within a solution of acrylic polymer with the weight ratio of iron oxide to acrylic polymer being within the range of from about 3:1 to 7:1 respectively; (B) forming a precursor filament by extruding

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗