US 4,099,996 A#47053920 Most CitedExpiredUnited States (USPTO)Utility

Process for heat-treating the head of railroad rail

1Forward Citations (#47053920 Global)
0.0/yrCitation Velocity (#59789928 Global)
1.01Citation PageRank (#40927559 Global)
4Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

In the process of heat-treating the head of a railroad rail wherein the rail is stressed so that the head forms a convex arc of predetermined height, the arc height is decreased about 14% after about 10% of the rail head has been heated, and then the original arc height is restored when about 40% of the rail head has been heated and then again decreased when about 60% of the rail head has been heated, and then finally the original arc height is again restored while the last 10% of the rail head length is heat treated.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    In the process for heat-treating a railroad rail having a head, web and flange wherein the rail is bent within the elastic limit in the plane of the web to form an arc having a predetermined height so that the head is convex and the flange concave, and the head of the rail is heat-treated progressively from one end to the other while holding the rail in such an arcuate condition, said heat treatment involving heating the rail head into the austenitic temperature range followed by a mild quench to form pearlite, the improvement comprising holding the rail in such predetermined arcuate condition