Patents
US 4,099,995 A#9836284 Most CitedExpiredUnited States (USPTO)Utility

Copper-hardened permanent-magnet alloy

10Forward Citations (#9836284 Global)
0.2/yrCitation Velocity (#31956911 Global)
3.88Citation PageRank (#4991533 Global)
6Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A copper-hardened permanent-magnet alloy consisting of cobalt, copper and at least one of the rare-earth metals (RE) with atomic number 57 - 71, is characterized by a coarse-grained matrix of the composition Re (Co 1-y Cu y ) 6+X , wherein 0≦X≦1 and 0.15<y<0.35.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 10.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A coarse-grained, copper-hardened permanent-magnet alloy having the formula Sm(Co.sub.1-y Cu.sub.y).sub.6+x, wherein 0 ≦ x ≦ 1, and 0.15 < y < 0.35, which is prepared by a process which comprises melting together the mixed components cobalt, copper, and samarium in weight proportions according to the final desired formula: holding the melt at a temperature of about 1400° C for from 3 to 5 minutes: and subsequently solidifying the melt in situ by applying a cooling rate of less than 50° C/min. within the solidification temperature range of between 1300° C and 1200° C.

  2. Claim 2Depends on #1

    The copper hardened permanent magnet alloy of claim 1, which has the approximate composition Sm(Co 1-y Cu y ) 6 , wherein 0.15 < y < 0.35.

  3. Claim 3Independent Claim

    T

Technical Overview & Description