US 4,098,731 A#837713 Most CitedExpiredUnited States (USPTO)Utility

Process for the production of foams

53Forward Citations (#837713 Global)
1.1/yrCitation Velocity (#5767827 Global)
7.94Citation PageRank (#1556453 Global)
10Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention relates to the production in closed molds, of foams with outstanding mold-release properties. These improved properties are obtained by including in the foamable mixture salts of saturated or unsaturated aliphatic or cycloaliphatic carboxylic acids having at least 8 carbon atoms and tertiary amines of the type in which the atom ratio of tertiary amine nitrogen to carbon in the molecule is between 1:3 and 1:12.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 53.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    In a process for the production of mold-formed foam having an impervious outer skin with self-releasing properties, said process comprising: (A) introducing a foamable reaction mixture into a closed mold, said mixture consisting essentially of: (i) an organic polyisocyanate, (ii) a compound having reactive hydrogen atoms and having a molecular weight of from 62 to 10,000, (iii) water and/or organic blowing agents, (iv) an isocyanate addition catalyst, and (v) an internal mold release agent, (B) allowing said foamable reaction mixture to foam in said mold, and (C) removing the res

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 53 total)

PatentTitleYearCitations
US 5,500,176 AProcess for the production of molded products using internal mold release agents199619
US 5,324,759 ARIM polyol blends containing acidic siloxane internal mold release agents and quaternary ammonium phenoxides19941
US 5,011,647 AInternal mold release compositions199116
EP 0,256,362 A3Process for the preparation of polyurethane and/or polyurea based mouldings and the mouldings obtained using this process—0
US 4,451,425 AMethod for injection molding polyurethane using internal release agents198417
US 5,208,268 AInternal release agents, active hydrogen containing mixtures which contain such agents and the use thereof in a process for the production of molded products199312
US 2011237770 A1Viscosity reducing agents for polyether polyols—4
US 4,965,293 APolyurea elastomers with improved surface quality19909
US 4,774,264 AProcess for the production of elastic molded articles198833
US 7,030,066 B1Wetting composition for high temperature metal surfaces, and method of making the same20060
US 4,609,682 AProcess for the production of moldings198622
US 11,112,103 B2In mold electronic printed circuit board encapsulation and assembly20210
US 5,158,607 AInternal release agents, active hydrogen containing mixtures which contain such agents and the use thereof in a process for the production of molded products199212
US 8,101,107 B2Method for producing pultruded components20127
US 4,936,917 AWater based mold release compositions containing poly(siloxane-glycol) surfactants for making polyurethane foam article in a mold199021