Roast-neutralization-leach technique for the treatment of laterite ore

39Forward Citations (#1431054 Global)
0.8/yrCitation Velocity (#9027890 Global)
16.07Citation PageRank (#481202 Global)
3Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method is provided for enhancing the neutralization capability of high-magnesium serpentine silicate ore in the neutralization of nickel-containing pregnant leach solution, said solution having a pH of less than about 1 which comprises, providing said high magnesium serpentine ore in particulate form containing by weight over about 5% magnesium, roasting said ore under oxidizing conditions at a temperature below that temperature at which forsterite in said ore recrystallizes, and then adding an amount of said serpentine roasted ore to said pregnant liquor sufficient to raise the pH of the leach solution to a level above 2.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 39.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    In a method of leaching a low-magnesium nickel-containing oxide ore, wherein an oxide ore containing by weight at least about 0.8% nickel and magnesium ranging up to about 5% is leached in a sulfuric acid solution at an elevated temperature exceeding about 150° C and an elevated pressure exceeding about 150 psig for a time sufficient to leach substantially the nickel therefrom and form a pregnant liquor thereof of pH less than about 1 and a leached residue, and wherein said pregnant liquor is neutralized by adding thereto a raw high-magnesium nickel-containing serpentine silicate ore containin

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 39 total)

PatentTitleYearCitations
CN 103,314,124 BFrom the method for material separation nickel with low nickel content20150
US 2011174113 A1Acid Recovery—8
US 5,571,308 AMethod for recovering nickel from high magnesium-containing Ni-Fe-Mg lateritic ore199696
RU 2,149,910 C1METHOD OF NICKEL RECOVERY FROM Ni-Fe-Mg LATERINE ORE WITH HIGH CONTENT OF MAGNESIUM20007
US 4,541,994 AMethod of liberating nickel- and cobalt-enriched fines from laterite198516
AU 705,253 B2Method for recovering nickel from high magnesium-containing Ni-Fe-Mg lateritic ore19990
CN 113,564,383 ASystem and process for extracting nickel and cobalt from laterite-nickel ore by two-stage pressurization—8
FR 2,549,492 A1Procede de recuperation du nickel a partir de minerais de laterites—1
WO 2012/080577 A1Method for separating nickel from material with low nickel content—0
WO 2009/132558 A1A method of extracting ni and/or co—1
WO 0,132,944 A1Method for leaching nickeliferous oxide ores of high and low magnesium laterites—36
US 2007034056 A1Process for recovery of nickel and cobalt by heap leaching of low grade nickel or cobalt containing material—5
US 2006024224 A1Method for nickel and cobalt recovery from laterite ores by combination of atmospheric and moderate pressure leaching—34
WO 0,250,321 A3Acid leaching of nickel laterite ores for the extraction of their nickel and cobalt values—0
CN 115,838,863 AMethod for synergistically extracting nickel and cobalt from limonite type laterite-nickel ore and saprolite type laterite-nickel ore—0