Patents
US 4,097,274 A#3605515 Most CitedExpiredUnited States (USPTO)Utility

Method of making superhard articles

22Forward Citations (#3605515 Global)
0.5/yrCitation Velocity (#17678151 Global)
4.99Citation PageRank (#3328840 Global)
3Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A superhard article is produced by heating in two steps a mixture of a hard-alloy matrix material and diamond grains less than 1 mm in size in a graphite press mould. During the first heating step, the mixture is heated to a temperature of 1,200° C at a rate of 1,000°-1,100° C per minute by heating the press mould by high frequency. During the second heating step, the mixture is heated to the sintering temperature, up to 1,800° C at a rate of 3,000°-10,000° C per minute by heating the mixture by the resistance method, i.e. by passing electric current through the mixture while simultaneously heating the press mould by high frequency currents.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 22.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of producing a superhard article comprising the steps of: charging a mixture of diamond grains less than 1 mm in size and a hard-alloy matrix material into a graphite press mould with the diamond grains being evenly distributed throughout the hard-alloy matrix material; heating the mixture under a pressure of from 50 to 100 kg/cm 2 to 1,200° C at a rate of from 1,000° to 1,100° C per minute by passing high frequency currents through the press mould; maintaining the mixture in the press mould at 1,200° C for less than 2 minutes to preclude graphitization and dissolution of the diamond

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 22 total)

PatentTitleYearCitations
US 5,169,572 ADensification of powder compacts by fast pulse heating under pressure199234
US 9,533,396 B2Polycrystalline ultra-hard material with microstructure substantially free of catalyst material eruptions20170
EP 1,028,171 A1Superhard composite material—13
FR 2,580,628 A1Diamond-contg. cobalt-cemented tungsten carbide prodn.—2
US 2010005728 A1Method for making composite abrasive compacts—16
EP 0,774,527 A3Superhard composite member and method of manufacturing the same—0
GB 2,433,525 BPolycrystalline ultra-hard material with microstructure substantially free of catalyst material eruptions20100
GB 2,472,931 APolycrystalline ultra-hard material formed in a two stage high temperature and high pressure process—0
US 2006015187 A1Pulsed current sintering for surfaces of medical implants—28
GB 2,472,931 BPolycrystalline ultra-hard material with microstructure substantially free of catalyst material eruptions20110
CN 110,152,558 ASintering device for superhard material and using method thereof—4
WO 2010/006064 A3Pulsed electrical field assisted or spark plasma sintered polycrystalline ultra hard material and thermally stable ultra hard material cutting elements and compacts and methods of forming the same—0
US 8,617,274 B2Pulsed electrical field assisted or spark plasma sintered polycrystalline ultra hard material and thermally stable ultra hard material cutting elements and compacts and methods of forming the same20135
CN 104,148,631 ASintering process of impregnated diamond bit—1
US 2010005729 A1Pulsed electrical field assisted or spark plasma sintered polycrystalline ultra hard material and thermally stable ultra hard material cutting elements and compacts and methods of forming the same—13