Patents
US 4,097,271 A#580908 Most CitedExpiredUnited States (USPTO)Utility

Hydrometallurgical process for recovering copper and other metal values from metal sulphides

64Forward Citations (#580908 Global)
1.3/yrCitation Velocity (#4189731 Global)
12.68Citation PageRank (#714863 Global)
10Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A hydrometallurgical process for the separate recovery of non-ferrous, ferrous, and precious metal values and sulfur from metal sulfide ore concentrates by leaching of metal sulfides with a lixiviant containing ferric chloride, cupric chloride and chlorine, precipitating cuprous chloride from the leach solution with butadiene, separating and decomposing the formed addition compound to recover the cuprous chloride, oxidizing and hydrolyzing the cuprous chloride to precipitate cupric oxychloride, converting the cupric oxychloride to cupric oxide, and reducing the cupric oxide with hydrogen for the recovery of copper. The leach residue is treated for the recovery of elemental sulfur and gold. Brine solution resulting from the conversion of cupric oxychloride to cupric oxide is electrolyzed for the production of sodium hydroxide for the cupric oxychloride conversion, hydrogen for the cupric oxide reduction and chlorine, which is partly used in the recovery of gold and partly recycled to the concentrate leach. Silver is recovered as silver iodide from the mother liquor from the cuprous chloride precipitation with butadiene. A portion of the solution from the silver recovery is treated f

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 64.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for the recovery of non-ferrous, ferrous and precious metal values and sulphur from concentrates containing metal sulphides which comprises the steps of: (1) subjecting said concentrates to a leach at a temperature in the range of about 80° to 110° C under autogenous pressure with lixiviant containing ferric chloride, cupric chloride and chlorine to form a leach solution containing cuprous chloride and a leach residue; (2) treating said leach solution with gaseous butadiene at a temperature in the range of about -35° to +40° C under autogenous pressure to form a precipitate of cupr

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗