US 4,095,544 A#1682566 Most CitedExpiredUnited States (USPTO)Utility

Production of corrosion resistant seam-free can bodies from tinplate

36Forward Citations (#1682566 Global)
0.8/yrCitation Velocity (#9832363 Global)
4.99Citation PageRank (#3330088 Global)
7Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

In the production of a seam-free can body from a sheet of flow brightened electrolytic tinplate by a method involving cold forming which includes a drawing step alone or a drawing step plus a redrawing step or plus a wall ironing step to produce a cold formed cup having inherently poor corrosion resistance, the improvement which comprises heat treating the cold formed cup at a temperature ranging from about 400 DEG to about 448 DEG F. for a period of time between about 10 minutes at the lower end of the temperature range and about 10 seconds at the upper end of the temperature range.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 36.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of producing a corrosion resistant seam-free can body comprising providing as a starting stock a planar sheet of steel of a thickness between about 0.025 inch and 0.005 inch having a coating of at least 1/4 lb. per BB of tin on each side and a layer of iron-tin alloy between the tin coating and the steel, the ATC value of at least one side of the tinplated steel being below 0.500 microamperes per cm 2 , subjecting the planar sheet of steel to a cold forming action, including a drawing step, to form a seamless cup having sidewalls, the steel of the sidewalls being subjected to plasti