Surface treatment with durable low-friction material

17Forward Citations (#5201304 Global)
0.3/yrCitation Velocity (#22259019 Global)
3.92Citation PageRank (#4927815 Global)
4Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present invention pertains to the treatment of a metal surface with a durable low-friction material in such a way as to greatly enhance the lubricant properties of the metal surfaces. The surface coating formed is a chromium plated surface containing microcracks so prepared as to permit injection or insertion of perfluorocarbon compositions such as polytetrafluoroethylene in a fused or nearly-fused state. In the method of forming the surface coating as described, the surface is plated by electrodeposition in a chromic acid bath followed by baking to oxidize the external plated surface. In this way, the surface may then be reverse etched to expand the microcracks without affecting the external surface, following which the plated surface may be heated to, or in excess of, the fusion point of the polytetrafluoroethylene material which is inserted preferably by application to the surface from a solid rod.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 17.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    The method of plating a metal surface comprising the steps of: (a) cleaning the metal surface; (b) electroplating the surface with chromium in a chromic acid bath to form a microcracked chromium plated surface portion; (c) heating the plated surface to oxidize the external surface thereof; (d) etching the plated surface to expand the cracks formed in the plating step; and (e) followed by applying a perfluorocarbon composition under pressure to fill the microcracks.

  2. Claim 2Depends on #1

    The method according to claim 1 in which the plated surface is baked during step (c) to a temperature on the order of 250° to 600° F within a period of one to five hours after plating.

  3. Claim 3Depends on #1

    The method according to claim 1 in which step (d) is further characterized by reverse etching of the plated surface to expand the microcracks formed in

Technical Overview & Description