US 4,094,692 A#28776908 Most CitedExpiredUnited States (USPTO)Utility

Process for stabilizing cement stone formed with aluminous binders

3Forward Citations (#28776908 Global)
0.1/yrCitation Velocity (#51626527 Global)
1.42Citation PageRank (#24837656 Global)
2Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Process for stabilizing cement stone, formed with binders rich in aluminates by setting with water, against high elevated temperatures and high humidity which comprises adding calcium sulfite to the aluminous binder material prior to setting. In another embodiment of the invention the addition of calcium borate along with the calcium sulfite provided even greater stability both initially and over a period of time. Calcium sulfite formed as a by-product of the waste gas purification of furnaces is the main source of supply for purposes of this invention.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 3.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    In a process wherein a cement stone-forming material is mixed with a binder rich in aluminates and with water, and is permitted to set to cement stone, the improvement which comprises adding calcium sulfite to said binder prior to said setting in an amount of at least 0.2 weight % up to about 10 weight % calculated as CaSO 3 based on the weight of said binder.

  2. Claim 2Depends on #1

    The process according to claim 1, wherein said calcium sulfite is added in an amount between about 0.2 and 5 weight %.

  3. Claim 3Depends on #1

    The process according to claim 1, wherein calcium borate is added in an amount between about 0.2 and 5.0 weight % based on the weight of said aluminous binder.

Technical Overview & Description