Abstract

The gold, silver and selenium content of copper refinery slimes are recovered by first leaching the slimes with dilute sulfuric acid at an elevated temperature and at a partial pressure of oxygen of between about 5 and 50 psig. to obtain a leach solution containing at least about 98% of the copper content of the raw slimes. The decopperized leach residue is dried and then roasted in an oxidizing atmosphere at a temperature of about 400° to 800° C. to obtain effluent roaster gases containing substantially all of the selenium content of the raw slimes in the form of selenium dioxide, the effluent roaster gases being treated to recover the selenium dioxide content thereof. The deselenized roaster residue is mixed with dilute acid and ferric chloride to form a slurry through which chlorine gas and air are continuously bubbled for a period of at least about 5 hrs. to obtain an extraction liquor containing the gold content and a chlorination residue containing the silver content of the raw slimes. The auric chloride-containing extraction liquor is then treated to recover the gold content thereof, and the silver chloride containing chlorination residue is treated to recover the silver con

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 53.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    Process for the recovery of gold, silver and selenium from copper refinery slimes containing these metals which comprises: treating the raw slimes with a dilute solution of sulfuric acid at a temperature of between about 40° and 100° C. and at a partial pressure of oxygen of between about 5 to 50 lbs. per square inch gauge to obtain a leach solution containing at least about 98% by weight of the copper content of the raw slimes and to obtain a decopperized leach residue containing the gold, silver and selenium content of the raw slimes, roasting the leach residue in an oxidizing atmpsphere a

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (2)