Anisotropic permanent magnet alloy and a process for the production thereof
Abstract
The thermo-magnetic-treated anisotropic permanent magnet alloy of the present invention consists essentially of, by weight, 17 to 45% chromium, 3 to 14.5% cobalt, 0.2 to 5% silicon and balance substantially iron, preferably 23 to 35% chromium, 7 to 14.5% of cobalt, 0.3 to 3% silicon and balance substantially iron and has a residual magnetic flux density of 7000 Gauss or more and a coersive force of 300 Oersted or more. In order to obtain the alloy, an alloy having the above identified composition is initially aged at a temperature of 570° C to 670° C for a period of 10 minutes to 5 hours in a magnetic field and secondarily aged at a temperature within 200° C below the thermo-magnetic treatment temperature for a period of 30 minutes to 50 hours.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 25.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A thermo-magnetic-treated anisotropic permanent magnet alloy having a residual magnetic flux density of 7,000 Gauss or more and a coercive force of 300 Oersted or more, said anisotropic permanent magnet alloy being prepared by subjecting an alloy consisting essentially of 17 to 45% by weight of chromium, 3 to 14.5% by weight of cobalt, 0.2 to 5% by weight of silicon and a balance of substantially iron to a solution treatment at 600° to 1300° C., heating the alloy in a magnetic field at a temperature of 570° to 670° C. for a period of 10 minutes to 5 hours, and then aging the thermo-magnetic tr
- Claim 2Depends on #1
The thermo-magnetic-treated anisotropic permanent magnet alloy as set forth in claim 1, wherein the anisotro