Patents
US 4,093,147 A#3192475 Most CitedExpiredUnited States (USPTO)Utility

Flat nylon 66 yarn having a soft hand, and process for making same

24Forward Citations (#3192475 Global)
0.5/yrCitation Velocity (#15152568 Global)
4.56Citation PageRank (#3856019 Global)
5Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Nylon 66 yarn having particular stress-strain properties, typically also having a soft, luxuriant hand in fabric form. As compared to conventional nylon 66 with comparable boiling water shrinkage, the novel yarn exhibits a higher modulus at break, a lower modulus at 10% elongation, a positive stress index, and excellent denier uniformity. The process involves subjecting the yarn, within 0.016 to 0.11 seconds after solidification of the filaments, to a tension of 0.2 and 1.5 grams per final denier and heating the yarn to a temperature between 50° and 250° C. long enough to reduce yarn retraction below 1%.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 24.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A bobbin having wound thereon a flat nylon 66 yarn having a substantially constant cross sectional configuration along its length, a shrinkage S less than 8.5%, an initial modulus greater than 15 g/d, a positive stress index ∝, and a retraction less than 1%.

  2. Claim 2Depends on #1

    The bobbin defined in claim 1, wherein said stress index ∝ exceeds 15.

  3. Claim 3Depends on #2

    The bobbin defined in claim 2, wherein said yarn has a 10% modulus less than 17 g/d.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Griehl et al., Faserforschung und Texliltechnils, 1, No. 6, (1958), pp. 226-231.