Patents
US 4,093,017 A#331322 Most CitedExpiredUnited States (USPTO)Utility

Cores for investment casting process

85Forward Citations (#331322 Global)
1.8/yrCitation Velocity (#2600384 Global)
13.60Citation PageRank (#636455 Global)
7Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A porous high-silica core is disclosed for use in directional solidification casting processes having exceptional thermal stability at temperatures above 1650° C. and containing mineralizers which promote the formation of cristobalite. The cores may be made by mixing at least 75 parts of essentially pure fused silica particles with 1 to 25 parts of activating particles containing a mineralizer, such as an alkali metal or alkaline earth metal compound, may be fired at a temperature of 1000° to 1300° C. until they contain 35 percent or more of cristobalite and may then be cooled to room temperature. They may thereafter be incorporated in a shell mold in accordance with the "lost-wax" process and preheated with the shell mold at a temperature of 1300° to 1600° C. to provide a cristobalite content of 60 to 85 percent or more within a short period of time, such as 10 to 30 minutes, and before a molten superalloy is allowed to flow into the mold. The core has exceptionally high thermal stability and may be maintained at a temperature of 1550° to 1600° C. or higher for one hour or more during the directional solidification process without substantial deformation. The high ultimate

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 85.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    In a directional solidification casting process for precision casting of superalloys wherein a molten metal alloy at a temperature above 1500° C. is caused to flow into a preheated multi-layer refractory shell mold containing a preformed porous leachable vitreous silica core body and is caused to solidify progressively from the bottom of the mold over a period of time, said shell mold and said core body being preheated to a temperature of from 1300° to 1600° C., the improvement which comprises providing the preformed core body with a mineralizer containing devitrifying metallic ions which prom

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗