Alkaline pulping of lignocellulosic material with amine pretreatment
Abstract
A lignocellulosic material, such as wood chips, is pretreated with an aqueous solution containing from 0.1 to 10% by weight of a water soluble lower aliphatic amine selected from monoethanolamine, methylamine and dimethylamine, at elevated temperature and pressure in a closed vessel. This pretreated material is then subjected to conventional soda or two-stage soda-oxygen pulping.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 19.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
In a process for pulping raw lignocellulosic material, the steps which comprise pretreating the lignocellulosic material with an aqueous solution containing from about 0.1 to 10% by weight of an aliphatic amine selected from monoethanolamine, methylamine and dimethylamine and thereafter subjecting the pretreated lignocellulosic material to digestion with sodium hydroxide alone at a sodium hydroxide application of at least 8% by weight expressed as sodium oxide based on the dry weight of said raw lignocellulosic material.
- Claim 2Depends on #1
A process according to claim 1 wherein the pretreatment is conducted at an amine solution to lignocellulosic material weight ratio of from 1:1 to 10:1 at a temperature of 80° to 180° C for 5 to 120 minutes.
- Claim 3Depends on #2
A process according to claim 2 wherein the pretreatment is conducted at a vessel pressure abo
Technical Overview & Description