Patents
US 4,090,874 A#3827790 Most CitedExpiredUnited States (USPTO)Utility

Method for improving the sinterability of cryogenically-produced iron powder

21Forward Citations (#3827790 Global)
0.4/yrCitation Velocity (#18140993 Global)
5.95Citation PageRank (#2495729 Global)
6Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method is disclosed of making sintered parts with cryogenically-produced powder derived from scrap metal, such as machine turnings. The scrap metal is subjected to two impacting operations (such as by use of a ball milling machine). The first operation is carried out with the use of a refrigerating agent (to lower the temperature of the scrap metal below its ductile-brittle transition temperature) thereby resulting in comminution of the scrap to a cryogenic powder. The second impacting operation is carried out at ambient temperature conditions utilizing milling elements which impart cold work to at least a portion of the cryogenic powder; simultaneously, copper is mechanically transferred to substantially each particle of said cryogenic powder to form a continuous copper envelope thereabout. The coated cryogenic powder is then compacted and sintered; the sintered product may be subjected to hardening or tempering treatments if desired.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 21.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A powder compact consisting essentially of a uniform and homogeneous mixture of ferrous-based first particles having a size range -200+325 mesh and containing oxidizable alloying ingredients including carbon, manganese and chromium and ferrous-based second particles having a size range of -60+140 mesh, one of said first and second particles having a copper envelope about substantially each of the particles thereof, and substantially each of the particles of said first particles having at least one impact stress defect site therein, said compact having a density of between 6.6-6.7 g./cc. and a

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 21 total)

PatentTitleYearCitations
US 2006198754 A1Method for preparing high-temperature nanophase aluminum-alloy sheets and aluminum-alloy sheets prepared thereby—14
US 5,296,189 AMethod for producing metal powder with a uniform distribution of dispersants, method of uses thereof and structures fabricated therewith199427
CN 102,277,510 AMixing method for preparation of diamond enhanced metal matrix composite material—7
US 5,441,579 AMethod of recycling scrap metal19956
EP 1,097,769 A1Method of manufacturing a preform or product from dispersion strengthened silver based alloys—3
US 7,354,490 B2Cryomilled aluminum alloys and components extruded and forged therefrom200814
US 2004228755 A1Cryomilled aluminum alloys and components extruded and forged therefrom—4
US 4,252,577 AMethod and apparatus for treating metal scrap cuttings198120
CN 102,277,510 BMixing method for preparation of diamond enhanced metal matrix composite material20120
US 2004065173 A1Method for preparing cryomilled aluminum alloys and components extruded and forged therefrom—22
US 5,152,847 AMethod of decarburization annealing ferrous metal powders without sintering19925
US 5,597,401 ARefractory metal SWARF composition and method of making same199713
US 6,902,699 B2Method for preparing cryomilled aluminum alloys and components extruded and forged therefrom200547
US 4,614,544 AHigh strength powder metal parts198614
US 5,292,477 ASupersaturation method for producing metal powder with a uniform distribution of dispersants method of uses thereof and structures fabricated therewith199418