Abstract

Flint is produced from a mischmetal and iron melt by permitting the alloy melt to cool in a mold at a slow enough rate that, as the solidification point of the melt is approached, its temperature is maintained at 800°-600° C for at least 10 minutes. The alloy melt is subsequently extruded and the extrudate is subjected to a heat treatment at temperatures from 370°-470° C for 1/2 to 4 hours, the heat treatment being discontinued before the limit value of the thermodynamic equilibrium has been reached.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 4.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of producing flint from a melt of a pyrophoric alloy of rare earth metals and iron, which comprises the steps of casting the alloy melt into a mold, permitting the melt to cool in the mold, slowing the cooling as the solidification point of the melt is approached sufficiently to maintain the alloy melt at a temperature from 770° to 610° C for a period of at least ten minutes, subsequently extruding the alloy melt and subjecting the extrudate to a heat treatment at temperatures from 370° to 470° C for one half hour to four hours, the heat treatment being discontinued before the limit v

  2. Claim 2Depends on #1

    The method of claim 1, wherein the alloy of rare earth me