US 4,088,732 A#8080253 Most CitedExpiredUnited States (USPTO)Utility

Improved method of beneficiating clay by removal of titanium and iron impurities

12Forward Citations (#8080253 Global)
0.2/yrCitation Velocity (#28166614 Global)
3.28Citation PageRank (#6546859 Global)
4Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of beneficiating kaolin clay by the addition of non-dispersing neutral salts to assist in the removal of discolored impurities, such as titanium and iron bearing minerals from a clay slurry. This process is capable of producing clays having a brightness in the 90- 95 range.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 12.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    An improved method for beneficiating an East Georgio kaolin clay, said method comprising the steps of: 1. treating an aqueous suspension of the kaolin clay be adding to the aqueous kaolin clay suspension a peptizing agent selected from the group consisting of polyphosphates, carbonates, silicates, alkalies, basic salts, and combinations thereof, in an amount in excess of that required to obtain minimum Brookfield viscosity of the kaolin clay-water-dispersant system as defined by measurement at 60% solids with a Brookfield viscometer at 10 r.p.m. using a No. 1 spindle; 2. further treating the