Polyphenylene sulphide applications
Abstract
A method of applying a bearing lining at least 0.005 inch thick of polyarylene sulphide to a bearing backing, which comprises applying to said backing a powder composition consisting of at least 80% by weight of uncured polyarylene sulphide together with at least 10% by weight of precured polyarylene sulphide, said precured polyarylene sulphide having been cured by being heated in air for 2 hours at at least 400° C and is in the form of particles with sizes in the range 53-211 microns, and then heating and curing the uncured polyarylene sulphide of the coating by heating to a temperature of at least 380° C. To produce the cured powder, uncured powder is mixed with salt and then cured; the salt prevents the powder from coalescing, and is subsequently dissolved out.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 11.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of applying a bearing lining at least 0.005 inch thick of polyarylene sulphide to a bearing backing, which comprises applying to said backing a powder composition consisting of at least 80% by weight of uncured polyarylene sulphide together with at least 10% by weight of precured polyarylene sulphide, said precured polyarylene sulphide having been cured by being heated in air for 2 hours at at least 400° C and is in the form of particles with sizes in the range 53-211 microns, and then heating and curing the uncured polyarylene sulphide of the coating by heating to a temperature of at
- Claim 2Depends on #1
A method as claimed in claim 1 in which the polyarylene sulphide is polyphenylene sulphide.
- Claim 3Depends on #1
A method as claimed in claim 1 in which the backing is coated in a fluidi