Photovoltaic cells
Abstract
A method of making low cost photovoltaic cells on a large scale basis by means of a continuous process of coating sheet glass while the sheet glass moves in and has its under surface immersed in a tank of molten material, comprising forming the film of CdS microcrystals on the glass sheet, which has previously been coated with transparent SnO x to a thickness of about 0.3 to 0.6 microns. A water solution of a cadmium salt, a sulphur compound, and an aluminum containing soluble compound is intermittenty sprayed on said glass while its exposed surface is maintained at a constant temperature in the range 500° F to 1100° F and while irradiating the surface with intense ultraviolet light so as to form a film of CdS microcrystals. This CdS film has Al impregnated within the stratum of the film adjacent to the SnO x , but only optionally has Al impregnated in the stratum of the CdS film adjacent to the exposed surface of the CdS film. After the spray process is completed, the temperature of the sheet of glass is brought to the range 450° C to 550° C, 525° being optium. After heating, the glass is cooled to approximately room temperature and the exposed surface of the CdS is converted to C
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 19.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of making a photovoltaic cell of the type having an insulating substrate, a first conductive layer, a second layer comprised of CdS, and a third layer forming a heterojunction with said second layer, comprising the step of forming at least a portion of said CdS layer with a composition comprising a cadmium salt, a sulphur containing compound, and an aluminum containing compound, the aluminum content of the composition being at least 10 molar percent of the total metal content of the composition.
- Claim 2Depends on #1
The method according to claim 1, further comprising the step of heat treating said CdS layer in an oxygen containing atmosphere at a temperature in the range 450° C to 550° C at some time prior to forming said third layer.
- Claim 3Depends on #1
The method according to claim 1, wherein said aluminum containing compound is AlCl 3 .
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗