Patents
US 4,085,236 A#11354107 Most CitedExpiredUnited States (USPTO)Utility

Process for producing electrostatic recording material

9Forward Citations (#11354107 Global)
0.2/yrCitation Velocity (#34528299 Global)
2.42Citation PageRank (#10689856 Global)
8Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process for producing an electrostatic recording material which comprises kneading a hydrophobic pigment having a critical surface tension of 50 dynes/cm or less with an aqueous dispersion of a copolymer consisting of (I) 10 to 50% by weight of methacrylic acid, (II) 5 to 50% by weight of a alkenyl aromatic compound and (III) 30 to 85 % by weight of at least one member selected from the group consisting of conjugated diolefins, alkyl acrylates and alkyl methacrylates; having a glass transition temperature (Tg) of 40 DEG C or less; and having an intrinsic viscosity [ eta ] of 0.1 to 1.0 dl/g as measured in tetrahydrofuran at 25 DEG C, in a weight ratio of the copolymer to the pigment of 100/20 to 100/200, in the presence of an alkaline material in such a proportion that the viscosity of the aqueous dispersion of the copolymer becomes at least 350 cps, adjusting the viscosity of the aqueous dispersion containing the copolymer and the hydrophobic pigment to 10 to 5,000 cps, coating the resulting coating composition on the surface of an electroconductive base sheet and drying the same. Said process can produce, with a high production efficiency, an electrostatic recording material ha

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 9.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for producing an electrostatic recording material which comprises kneading a hydrophobic pigment having a critical surface tension of 50 dynes/cm or less with an aqueous dispersion of a copolymer consisting of (I) 10 to 50% by weight of methacrylic acid, (II) 5 to 50% by weight of an alkenyl aromatic compound and (III) 30 to 85% by weight of at least one member selected from the group consisting of conjugated diolefins, alkyl acrylates, and alkyl methacrylates; having a glass transition temperature (Tg) of 40° C or less; and having an intrinsic viscosity [η] of 0.1 to 1.0 dl/g as mea

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗