Method for providing environmentally stable aluminum surfaces for adhesive bonding and product produced
Abstract
Environmentally stable bond joints of aluminum metal and aluminum alloys in adhesively joined structures are formed by utilizing a prebonding anodization of the aluminum surfaces in a phosphoric acid electrolyte containing from about 1.5 to about 50% H 3 PO 4 at 1 to 50 volts for a period of 5 to 60 minutes using a bath temperature of 50° to 100° F. The anodized surface is then washed free of electrolyte, dried and coated with an adhesive resin. The aluminum metal segments are then arranged in a composite arrangement and bonded together under pressure and heat to cure the adhesive resin. The resulting structure is resistant to failure of the bond joints on exposure to moist atmospheric conditions. The surface preparation provides a hydration resistant aluminum oxide surface which minimizes adhesive-aluminum separation under aqueous exposure. Alloys containing copper and other alloying constituents may be successfully anodized and bonded by this process.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 55.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of preparing an adhesively bonded aluminum structure comprising forming a porous columnar aluminum oxide coating on surfaces of aluminum alloy articles, said aluminum alloy articles containing about 1.6 to about 4.5% by weight copper by anodizing said articles in an aqueous solution comprising phosphoric acid, the anodizing potential being from about 3 to about 25 volts, the phosphoric acid concentration being about 3 to about 20% by weight and the temperature of said solution being from about 50° F. to about 85° F.; rinsing said articles to remove said solution; applying an adhes
- Claim 2Depends on #1
The method of claim 1 wherein said alumimum alloy article consists of aluminum alloy 7075. --
- Claim 3Depends on #1
The method of claim 1
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 55 total)
References Cited — Backward Prior Art (8)
Non-Patent Literature (3)
- "American Wrought Alloys", Aluminum, S. Wernick, 1964, p. 759.
- "The Surface Treatment and Finishing of Al", by Wernick et al., 3rd Ed., 1964, pp. 284-286.
- Surface Treatment of Al by Wernick et al., 3rd Ed., 1964, p. 759.